MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Eastek™ 1200 Polymer Dispersion
Categories: Polymer

Material Notes: Product Description: Eastek™ 1200 polymer dispersion is a film forming polyester polymer supplied as an aqueous solution containing 2% n-propanol and 30% polymer solids. Eastek™ 1200 provides excellent water resistance, alcohol resistance, fast drying rates, low odor, and a consistently low coefficient of friction. Eastek™ 1200 polymer dispersion is amine and surfactant free.

Application/Uses:

  • Overprints
  • Primers for industrial wood coatings
  • Printing Inks

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 30 %
Brookfield Viscosity 100 cPModel DV II, using Spindle 2 @ 60 rpm
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 63.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, Cast
Precision Polymer Engineering N80X Nitrile Rubber
Eastman AQ™ 65S Polymer
Chevron Phillips Marlex® 5104 LDPE Blow Molding Resin
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded

PEATM5116 / 222310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.