MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sawbones Cellular Rigid Polyurethane Foam 20 pcf Density
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Cellular Rigid Polyurethane Foam

Primary Use
Cellular rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. Its outward appearance matches cancellous bone more closely than solid rigid polyurethane foam products, however they provide a somewhat less consistent and uniform test bed.

Description
The appearance of cellular rigid polyurethane foam resembles that of cadaveric cancellous bone, however, the cell structure is 95% closed as compared to the open cell structure of cancellous bone. Foam is available in a range of sizes and densities, from 0.12 to 0.32 grams per cubic centimeter (7.5 to 20 pounds per cubic foot) and cell sizes ranging from 0.5 to 1.0 mm.

Information provided by Sawbones.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 g/cc
 
Mechanical PropertiesOriginal ValueComments
Compressive Yield Strength 5.40 MPa
Compressive Modulus 0.1375 GPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sawbones Solid Rigid Polyurethane Foam 20 pcf Density
Sawbones Solid Rigid Polyurethane Foam 50 pcf Density
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density
Sawbones Second-Generation Simulated Cancellous Bone (Solid)
Sawbones Second-Generation Simulated Cancellous Bone (Cellular)

PSAWBO09 / 66540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.