Crosslinked silicone adhesive with polyester film and crepe paper backing. Features: - High temperature resistant
- No adhesive residue even when there is a delay between wave soldering and tape removal
- Good conformability
Applications: For protecting gold finger contacts during wave soldering and hot air leveling of PCBs. Information provided by Dielectric Polymers. |