System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
3M 9731 Double Coated Tape
Categories:
Polymer
;
Adhesive
Material Notes:
3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other side of the carrier.
Information provided by 3M
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Thickness
25.4
microns
1.00
mil
Carrier
40.6
microns
1.60
mil
Faceside Adhesive
73.7
microns
2.90
mil
Backside Adhesive
73.7
microns
2.90
mil
Backside Liner
107
microns
4.20
mil
Faceside Liner
140
microns
5.50
mil
Total Thickness
Mechanical Properties
Metric
English
Comments
Peel Strength
0.42729
kN/m
2.4375
pli
ABS, 180°, 2 mil al foil, Silicone Adhesive, 72 hr RT; ASTM D3330
0.438
kN/m
2.50
pli
Stainless Steel, 90°, Silicone Adhesive, 15 min RT; ASTM D3330
0.438
kN/m
2.50
pli
Polypropylene, 180°, 2 mil al foil, Silicone Adhesive, 72 hr RT; ASTM D3330
0.4602
kN/m
2.625
pli
Stainless Steel, 90°, Silicone Adhesive, 72 hr RT; ASTM D3330
0.4602
kN/m
2.625
pli
Polycarbonate, 180°, 2 mil al foil, Silicone Adhesive, 72 hr RT; ASTM D3330
0.482
kN/m
2.75
pli
Polypropylene, 180°, 2 mil al foil, Acrylic Adhesive, 72 hr RT; ASTM D3330
0.526
kN/m
3.00
pli
Stainless Steel, 90°, Silicone Adhesive, 72 hr at 150°F; ASTM D3330
0.657
kN/m
3.75
pli
Polycarbonate, 180°, 2 mil al foil, Acrylic Adhesive, 72 hr RT; ASTM D3330
0.77789
kN/m
4.4375
pli
Stainless Steel, 90°, Acrylic Adhesive, 15 min RT; ASTM D3330
0.8108
kN/m
4.625
pli
ABS, 180°, 2 mil al foil, Acrylic Adhesive, 72 hr RT; ASTM D3330
1.0189
kN/m
5.8125
pli
Stainless Steel, 90°, Acrylic Adhesive, 72 hr RT; ASTM D3330
1.3257
kN/m
7.5625
pli
Stainless Steel, 90°, Acrylic Adhesive, 72 hr at 150°F; ASTM D3330
Electrical Properties
Metric
English
Comments
Electrical Resistivity
2.60e+15
ohm-cm
2.60e+15
ohm-cm
Silicone Adhesive Surface
3.40e+15
ohm-cm
3.40e+15
ohm-cm
Volume
7.40e+15
ohm-cm
7.40e+15
ohm-cm
Acrylic Adhesive Surface
Dielectric Strength
315
kV/mm
8000
kV/in
ASTM D1000
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
121
°C
250
°F
Long term
177
°C
351
°F
Short term
Processing Properties
Metric
English
Comments
Shelf Life
18.0
Month
18.0
Month
Descriptive Properties
Appearance
Backside liner
Faceside Liner
Liner
Fluoropolymer non-silicone clear, PET
Tan, Polycoated Kraft
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Solvay Flashtape 1R Adhesive tape
3M XG6110 General Purpose Double Coated Tape
3M F-9465PC Adhesive Transfer Tape
3M ATG 924 Tape
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE
PMM33288 / 168035
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.