INNOPOL® CS 3-9120 SR5 is a 17% talc-filled compound based on blend of polypropylene block copolymer and homopolymer. This grade is available in natural and custom colored form. INNOPOL® CS 3-9120 SR5 is developed for producing injection molded automotive components. Information provided by INNO-COMP |