MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

TSRC Taipol® 1453 SSBR
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Polymerization System: Solution Polymerization, styrene butadiene random copolymer

Stabilizer: Non-Staining

Characteristics: High strength, better resilience and rolling resistance

Application: Tire, footwear and industrial goods

Test Recipe
SSBR-1453 – 100
N330 - 50
Dark oil - 10
Wax – 1.5
S.A – 2
ZnO – 4
A.O (3C) – 1
CZ – 1
S – 1.75
Total – 171.25

Information provided by TSRC Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.0 %<= 1.0 %K62-TPFP-01
Mooney Viscosity 49 - 6149 - 61ML1+4; ASTM D-1646
Ash <= 0.50 %<= 0.50 %ASTM D-5667
 
Chemical PropertiesMetricEnglishComments
Styrene Content 9.0 - 11 %9.0 - 11 %Bound; K62-TPPC-21
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 9.81 MPa>= 1420 psiCure @ 35 min for 145?; ASTM D-412
Elongation at Break >= 300 %>= 300 %Cure @ 35 min for 145?; ASTM D-412
 
Descriptive Properties
1,2-Vinyl0.4K62-TPPC-21

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTSRC009 / 306297

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.