MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik VESTODUR® X7212 black E70149 Polybutylene Terephthalate  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled

Material Notes: Self-extinguishing, reinforced polybutylene terephthalate compound with non-migrating and non-corrosive flame retardant. VESTODUR® X7212 black E70149 is a glass fiber-reinforced (45%), semi-crystalline thermoplastic compound for injection molding, based on polybutylene terephthalate (PBT).
VESTODUR® X7212 is used for parts of high mechanical and thermal resistance. Test bars made of the compound are rated V-0 self-extinguishing according to UL94 by Underwriters Laboratories Inc. The incorporated flame retardant is non-migrating. The additive has no corrosive effects on metal inserts or neighboring metal parts. Therefore, the compound is distinguished for moldings in the electrical and electronical industry. Laser marking with high contrasts is possible. VESTODUR® X7212 is supplied as cylindrical pellets in polyethylene packaging. Pigmentation may affect values.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.84 g/ccISO 1183
Water Absorption 0.30 %Sim. to ISO 62
Moisture Absorption 0.0100 %ISO 15512
Linear Mold Shrinkage 0.0070 cm/cmNominal; ISO 294-4, 2577
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4, 2577
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86
@Time 3.00 sec
ISO 7619-1
Tensile Strength at Break 150 MPaISO 527
Elongation at Break 1.3 %ISO 527
Tensile Modulus 15500 MPaISO 527
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eU
 48.0 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+13 ohmRSD; IEC 62631-3-2
Dielectric Constant 4.4
@Frequency 100 Hz
IEC 62631-2-1
 4.6
@Frequency 1e+6 Hz
IEC 62631-2-1
Dielectric Strength 31.0 kV/mmAC, S20/P50; Sim. to IEC 60243-1
Dissipation Factor 0.0040
@Frequency 100 Hz
IEC 62631-2-1
 0.013
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 250 Vtest solution A, 100 drops value; IEC 60112
 275 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 40.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 224 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 223 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 217 °CISO 75-1/-2
Vicat Softening Point 215 °CMethod B: 10 N, 50 K/h; ISO 306
 220 °CMethod A: 10 N, 50 K/h; ISO 306
Glass Transition Temp, Tg 45.0 °CISO 11357-1/-2
Flammability Test 5.0UL 94
 5.0
@Thickness 0.400 mm
IEC 60695-11-10
 5.0
@Thickness 0.800 mm
IEC 60695-11-10
 5.0
@Thickness 1.60 mm
IEC 60695-11-10
Oxygen Index 37 %ISO 4589-1/-2
Glow Wire Ignition Temperature 775 °CIEC 60695-2-13
Glow Wire Flammability Index 960 °CIEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CTest condition for mold shrinkage
Mold Temperature 80.0 °CTest condition for mold shrinkage

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK887 / 243094

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.