MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Plyophen 23900 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: DESCRIPTION: Plyophen 23900 is a liquid one-step phenolic resin in ethanol.

APPLICATION: Plyophen 23900 is a heat resistant laminating varnish. This resin is a high heat resistant, low or high pressure, laminating phenolic with exceptionally high strengths at elevated temperatures. It is generally reinforced with glass cloth or glass filaments, but can also be reinforced with other materials. The preimpregnation of reinforcements with this resin is quite simple, and the resin content and volatile content can be easily adjusted for the particular application.

Laminates made with this resin, in addition to the high physical properties at elevated temperatures, have good resistance to organic solvents, weak inorganic acids, and hydraulic aircraft oil or de-icing fluids, low moisture absorption, and good resistance to rain and hot gas erosion.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccDCT 5075
Viscosity 100 cP
@Temperature 25.0 °C
DCT 4003F
 
Descriptive Properties
ColorClearDCT 0001
Non Volatile (%)64DCT 5009

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® P23056NF Phenolic Resin
Sumitomo Bakelite North America Epiall® 1960B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Sumitomo Bakelite North America Epiall® 1914A Short Glass Fiber Reinforced Epoxy
Sumitomo Bakelite North America CF 9040A Carbon Fiber Reinforced Phenolic
Sumitomo Bakelite FM 4005X4648 Phenolic Novolac Molding Compound

PSUMIT182 / 193987

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.