MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Haysite Thermalate® H320 Glass Mat Reinforced Polyester Laminate
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: Platen Insulation. A tough and durable composite with high compressive strength and resistance to oil and fluid absorption. Recommended for use in operating temperatures up to 450 F, this material used as press insulation will result in energy and maintenance savings. Standard color is brown.

Key Words: Fiberglass
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.18 %0.18 %3/8" Sanded; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 159 MPa23100 psi
Compressive Strength 305 MPa44200 psi
Izod Impact, Notched 5.30 J/cm9.93 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 24.0 µm/m-°C
@Temperature 20.0 °C
13.3 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 232 °C450 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haysite Thermalate® H330 Glass Mat Reinforced Polyester Laminate
A. Schulman Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass
Röchling Glastic Laminates/Shapes TSF Fiberglass-Reinforced Polyester Laminate

PHAY26 / 45632

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.