MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Elvax® 40L-03 Low Smoke Non-halogen Jacket Formulation  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Elvax® 40L-03 low smoke non-halogen jackets.

Information provided by DuPont.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 39
@Temperature 100 °C
39
@Temperature 212 °F
ML 1 + 4; ASTM D1646
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 12.0 MPa1740 psiExtruded wire; ASTM D412
 13.2 MPa1910 psiAfter 7 days/150°C air oven, ASTM D573
 10.32 MPa
@Treatment Temp. 121 °C,
Time 64800 sec
1497 psi
@Treatment Temp. 250 °F,
Time 18.0 hour
in ASTM #2 Oil
Elongation at Break 173.8 %173.8 %After 7 days/150°C air oven; ASTM D573
 220 %220 %Extruded wire; ASTM D412
 149.6 %
@Treatment Temp. 121 °C,
Time 64800 sec
149.6 %
@Treatment Temp. 250 °F,
Time 18.0 hour
in ASTM #2 Oil
Tear Strength 7.00 kN/m39.9 pliASTM D470
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -35.0 °C-31.0 °FASTM D746
Smoke Density <= 23<= 23Flaming Mode, NBS; ASTM E662
 <= 146<= 146NBS Non-Flaming Mode; ASTM E662
Oxygen Index 32 %32 %ASTM D2863
 
Descriptive Properties
a,a'-bis [t-butylperoxy] diisopropylbenzene2.5 phr
Antioxidant1.5 phr
Elvax® 40L-03100 phr
HVA-21 phr
Hydrated Alumina150 phr
Silquest A-172.75 phr
SRF Carbon Black5 phr
Stearic Acid1 phr
Volume Swell (%)58After 18hr/121°C in ASTM #2 Oil
 90After 70hr/100°C in ASTM #3 Oil

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Elvax® 40L-03 High Temperature Ignition Cable Jacket Formulation
Dow Elvax® 40L-03 Ethylene-Vinyl Acetate Copolymer Resin
DuPont Elvax® 3130SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
DuPont Elvax® 3130SBZ Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
DuPont Elvax® 3134Q Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating, Casting

PDUPM116 / 33783

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.