MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPE RV-2668DN Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink RV-2668DN is a high performance thermoplastic elastomer used in transportation applications. Sarlink RV-2668DN is a high hardness grade and UV resistant. This grade can be processed by extrusion and injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Filled; Good Adhesion; Light Stabilized; Medium Density; Low Flow; High Hardness; Sunlight Resistant; Slip

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; General Purpose; Grommets; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Viscosity 560 cP
@Shear Rate 206 1/s,
Temperature 200 °C
560 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  68
@Time 15.0 sec
68
@Time 0.00417 hour
Injection Molded; ISO 868
 69
@Time 5.00 sec
69
@Time 0.00139 hour
Injection Molded; ISO 868
 73
@Time 1.00 sec
73
@Time 0.000278 hour
Injection Molded; ISO 868
 69.3
@Treatment Temp. 125 °C,
Time 15.0 sec
69.3
@Treatment Temp. 257 °F,
Time 0.00417 hour
Change in Air, 168 hr; ISO 888
 70.2
@Treatment Temp. 125 °C,
Time 5.00 sec
70.2
@Treatment Temp. 257 °F,
Time 0.00139 hour
Change in Air, 168 hr; ISO 888
 70.3
@Treatment Temp. 110 °C,
Time 15.0 sec
70.3
@Treatment Temp. 230 °F,
Time 0.00417 hour
Change in Air, 1008 hr; ISO 888
 71
@Treatment Temp. 110 °C,
Time 5.00 sec
71
@Treatment Temp. 230 °F,
Time 0.00139 hour
Change in Air, 1008 hr; ISO 888
 74.1
@Treatment Temp. 125 °C,
Time 1.00 sec
74.1
@Treatment Temp. 257 °F,
Time 0.000278 hour
Change in Air, 168 hr; ISO 888
 75
@Treatment Temp. 110 °C,
Time 1.00 sec
75
@Treatment Temp. 230 °F,
Time 0.000278 hour
Change in Air, 1008 hr; ISO 888
Tensile Strength at Break 21.8 MPa3160 psiAcross Flow, Type 1, 20 in/min; ISO 37
 25.1 MPa3640 psiFlow, Type 1, 20 in/min; ISO 37
 21.2 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
3070 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Type 1, Change in Air; ISO 188
 22.2 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
3220 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Type 1, Change in Air; ISO 188
 25.7 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
3730 psi
@Treatment Temp. 257 °F,
Time 168 hour
Flow, Type 1, Change in Air; ISO 188
 27.1 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
3930 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain  14.5 MPa
@Strain 100 %
2100 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 14.8 MPa
@Strain 100 %
2150 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 16.6 MPa
@Strain 100 %,
Treatment Temp. 110 °C
2410 psi
@Strain 100 %,
Treatment Temp. 230 °F
Across Flow, Type 1, Change in Air, 1008 hr; ISO 188
 17.0 MPa
@Strain 100 %,
Treatment Temp. 125 °C
2470 psi
@Strain 100 %,
Treatment Temp. 257 °F
Across Flow, Type 1, Change in Air, 6.61 in; ISO 188
 24.3 MPa
@Strain 100 %,
Treatment Temp. 110 °C
3530 psi
@Strain 100 %,
Treatment Temp. 230 °F
Flow, Type 1, Change in Air, 1008 hr; ISO 188
 25.3 MPa
@Strain 100 %,
Treatment Temp. 125 °C
3680 psi
@Strain 100 %,
Treatment Temp. 257 °F
Flow, Type 1, Change in Air, 168 hr; ISO 188
Elongation at Break 140 %140 %Flow, Type 1, 20 in/min; ISO 37
 320 %320 %Across Flow, Type 1, 20 in/min; ISO 37
 130 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
130 %
@Treatment Temp. 230 °F,
Time 1008 hour
Flow, Type 1, Change in Air; ISO 188
 134 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
134 %
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Type 1, Change in Air; ISO 188
 147 %
@Treatment Temp. 125 °C,
Time 605000 sec
147 %
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Type 1, Change in Air; ISO 188
 178 %
@Treatment Temp. 125 °C,
Time 605000 sec
178 %
@Treatment Temp. 257 °F,
Time 168 hour
Flow, Type 1, Change in Air; ISO 188
Tear Strength 140 kN/m800 pliFlow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
 210 kN/m1200 pliAcross Flow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
Compression Set  63 %
@Temperature 22.8 °C,
Time 79200 sec
63 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ISO 815
 86 %
@Temperature 70.0 °C,
Time 79200 sec
86 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ISO 815
 93 %
@Temperature 90.0 °C,
Time 252000 sec
93 %
@Temperature 194 °F,
Time 70.0 hour
Type 1; ISO 815
 100 %
@Temperature 125 °C,
Time 252000 sec
100 %
@Temperature 257 °F,
Time 70.0 hour
Type 1; ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 188 - 210 °C370 - 410 °FInjection, Melt
Rear Barrel Temperature 171 - 193 °C340 - 380 °FInjection
Middle Barrel Temperature 177 - 199 °C350 - 390 °FInjection
Front Barrel Temperature 182 - 204 °C360 - 400 °FInjection
Nozzle Temperature 188 - 210 °C370 - 410 °FInjection
Zone 1 166 - 188 °C330 - 370 °FExtrusion
Zone 2 171 - 193 °C340 - 380 °FExtrusion
Zone 3 177 - 199 °C350 - 390 °FExtrusion
Zone 4 191 - 210 °C375 - 410 °FExtrusion
Zone 5 182 - 204 °C360 - 400 °FExtrusion
Die Temperature 190 - 210 °C374 - 410 °FExtrusion
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceNatural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1127 / 237618

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.