MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese Ateva® 1880A Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Ateva® 1880A resin is suitable for use in hot melt coating and adhesive applications, as well as carpet extrusion coating applications. It contains an antioxidant to minimize viscosity changes of the hot melt blends during processing. It complies with Code of Federal Regulation 21 CFR Section 177.1350 and 175.105, subject to extraction limitations for specific end use applications. This polymer may be processed on conventional extrusion equipment. It is recommended that the melt temperature be kept below 210°C as decomposition can occur at higher temperatures. Additives: Antioxidant

Applications: Adhesives & Sealants; Automotive

Information provided by Celanese Corporation.

Key Words: hot melt coating and adhesive applications as well as carpet extrusion coating applications
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D1505; ASTM D1928 Proc A
Vinyl Acetate Content 18 %18 %AT Plastics PTM-39
Melt Flow 500 g/10 min
@Load 0.325 kg,
Temperature 125 °C
500 g/10 min
@Load 0.716 lb,
Temperature 257 °F
Modified; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
Tensile Strength at Break 4.00 MPa580 psiType IV (50 mm/min); ASTM D638
Elongation at Break 570 %570 %Type IV (50 mm/min); ASTM D638
Flexural Modulus, 1% Secant 31.0 MPa4500 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Ring & Ball Softening Point 89.0 °C192 °FASTM E28
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Petroquimica Triunfo Tritheva® PN 2021 EVA Copolymer
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer
Celanese Ateva® 2842A Ethylene Vinyl Acetate Copolymer
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend
Celanese Ateva® 2830A Ethylene Vinyl Acetate Copolymer

PATEVB05 / 25961

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.