MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Rondo Plast REPRO ABS RE5 Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Standard injection moulding

Information provided by Rondo

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inISO 2577
Melt Flow 12 g/10 min
@Load 5.00 kg,
Temperature 230 °C
12 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 30.0 MPa4350 psiISO/R 527
Flexural Strength 70.0 MPa10200 psiISO 178
Flexural Modulus 2.10 GPa305 ksiISO 178
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.0 °C
@Load 5.001 kg
194 °F
@Load 11.03 lb
ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Glow Wire Ignition Temperature 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
IEC 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRNDP007 / 280793

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.