MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Syndustrial® Hydraulic Fluid ISO Grade 32
Categories: Fluid; Lubricant

Material Notes: Phillips 66® Syndustrial Hydraulic Fluid is a premium quality, synthetic anti-wear hydraulic fluid specifically developed for use in industrial and mobile equipment operating in environmentally sensitive areas. It is readily biodegradable for reduced environmental impact in case of leaks or spills. Three grades are certified by the FMRC as fire-resistant for use in areas subject to fire hazards, and two grades are approved by the MSHA for use in underground mining equipment. Syndustrial Hydraulic Fluid is formulated with synthetic polyolester (POE) base oil and select ashless additives to provide excellent lubrication and wear protection for hydraulic pumps and motors. It also protects hydraulic system components against rust and corrosion. It has outstanding oxidation resistance and thermal stability at high temperatures, plus excellent detergency, to protect against sludge and varnish formation, and provide long service life. It is readily biodegradable as determined by the OECD 301C test method. It passes the visual “no sheen” requirements of the U. S. EPA Static Sheen Test. The ISO 46, 68, and 100 viscosity grades are especially recommended for use in equipment operating in areas subject to fire hazards, such as steel mills, surface mines, and foundries. All three grades are approved by Factory Mutual Research Corporation (FMRC) as less flammable hydraulic fluids. The ISO 68 & 100 viscosity grades also are approved by the MSHA for use in underground mining equipment. Syndustrial Hydraulic Fluid does not contain water, mineral oil, or phosphate ester. It may be used in hydraulic systems designed for conventional mineral oil-based hydraulic fluids without compromising overall hydraulic system integrity. However, it should not be mixed with other fluid types. When converting from water-glycol fluids, invert emulsions, or phosphate esters, the system should be flushed prior to conversion, and seal compatibility should be verified.

Applications:

  • Mobile and stationary equipment operating in environmentally sensitive areas (all grades)
  • Hydraulic systems subject to fire hazards and/or extreme heat (ISO VG 46, 68,100)
  • Steel mill, foundries, and manufacturing plants (ISO VG 46, 68, 100)
  • Underground mining equipment where a fire-resistant, MSHA-approved hydraulic fluid is required (ISO VG 68, 100)
Syndustrial Hydraulic Fluid meets the requirements of the following test:
  • U.S. EPA/Coast Guard Static Sheen Test, Federal Register Vol. 58, No. 41
Syndustrial Hydraulic Fluid is approved as meeting the requirements of the following industry specification:
  • Factory Mutual Group II, Type HFD-U (ISO 6743-4), Less Flammable Hydraulic Fluid (ISO VG 46, 68, 100)
Features/Benefits:
  • Fire resistant, with high flash point, fire point, and auto-ignition temperature for reduced risk of fire/explosion (ISO 46, 68, 100)
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • Excellent wear protection for hydraulic pumps and motors
  • Protects against rust and corrosion
  • Good low-temperature fluidity
  • Non-toxic, non-irritating, and contains no hazardous ingredients
  • Readily biodegradable (all grades)
  • Fire resistance certified by Factory Mutual Research Corporation (ISO 46, 68, 100)
  • MSHA approved (Approval Number 35-A080004, ISO VG 68; Approval Number 30-20-3, ISO VG 100)

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.948 g/cc
Density 7.90 lb/gal
Viscosity Measurement 166Index
Saybolt Viscosity at 100°F 151 SUS
Saybolt Viscosity at 210°F 46.9 SUS
Kinematic Viscosity at 40°C (104°F) 29.6 cSt
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.30[mg KOH/g]; ASTM D974
 
Thermal PropertiesOriginal ValueComments
Pour Point -49.0 °C
Flash Point 270 °CCOC
 
Descriptive Properties
Biodegradability>70%OECD 301C, 28 days
ColorLight Amber
Copper Corrosion1bASTM D130, 48 hrs @ 80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phillips 66 Quintolubric® 958-30 Hydraulic Fluid
Shin-Etsu Silicones KF-54 Fluid
Phillips 66 Synjex® TC-W3® 2-Cycle Motor Oil
Phillips 66 Megaplex® XD5 NGLI Grade 1
Nye Lubricants 415 (SO) Synthetic Oil

WCON5436 / 198689

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.