MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Glyptal C1815B Alkyd Primer
Categories: Polymer; Thermoset; Alkyd

Material Notes: GLYPTAL C-1815B beige air-dry waterborne alkyd primer is designed for single-coat application on industrial components subject to exterior exposure. C-1815B will demonstrate rapid dry-to-handle characteristics. The dried film will exhibit excellent early hardness and handling capabilities while continuing use in atomic power installation where a minimum level of trace elements is required.

C1815B fast, air-dry alkyd primer is recommended for use on clean, prepared steel where fastdry and excellent corrosion resistance is required. Application may be accomplished with traditional spray equipment with no extraordinary requirements in terms of peripherals and technique. pH and freeze/thaw stability are excellent requiring only that the material be maintained under normal ambient conditions.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³
Solids Content 29 - 33 %29 - 33 %Volume
 44 - 48 %44 - 48 %Weight
Fineness >= 6.5>= 6.5Hegman
pH 8.4 - 8.68.4 - 8.6
Thickness 25.4 - 76.2 microns1.00 - 3.00 milDry Film
 
Thermal PropertiesMetricEnglishComments
Flash Point 95.0 °C203 °Fcc/pm
 
Optical PropertiesMetricEnglishComments
Gloss 5.0 - 10 %5.0 - 10 %60°
 
Processing PropertiesMetricEnglishComments
Dry Time 1.00 - 1.50 hour1.00 - 1.50 hourHandle
 48.0 - 72.0 hour48.0 - 72.0 hourFull Hardness
Cure Time 30.0 - 60.0 min0.500 - 1.00 hourTackfree
 
Descriptive Properties
Adhesion1Cross Hatch
Chemical Resistance>200 hoursHumidity
 200 hoursSalt Fog
ColorBeige
Coverage502 ft²/gal1 mil dry film thickness
FlexibilityPass
MethodSpray
ReducerWaterIf necessary
SubstrateShot Blasted
Viscosity80-90 KU

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyester (Thermoset) - Rigid
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Overview of materials for Melamine-Phenolic Copolymer
Overview of materials for Epoxy Adhesive
Overview of materials for ABS/Polyester Alloy

PGLYPT925 / 209764

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.