MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Evonik VESTANAT® EP-M 95 Polyisocyanate
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: This product is a silane functional crosslinker for curing at elevated temperatures used in combination with suitable binders. It can be used for the formulation of highly scratch resistant coatings. For best results the coating requires a catalyst such as VESTANATR EP-CAT 11. The product is also suitable as a booster for scratch resistance for stoving emanels (plug-in technology). VESTANATR EP-M 222 can be added to adjust flexibility of finished coatings.

Benefits:

  • Outstanding scratch resistance
  • Solvent free (VESTANATR EP-M 95)
  • Excellent chemical resistance
  • Scratch resistance “booster” for stoving enamels

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 500 - 700 cP
 
Descriptive Properties
Color<50Hazen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-6710 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3703 Polyurethane Foam
Covestro Baytuft® 752A Polyurethane
Covestro Bayfill® 310 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 20 pcf, MDI-based 2-Component Liquid System

PEVONIL337 / 196541

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.