MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® DX9325 BK E70352 Nylon 612, 40% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Glass Fiber Filler

Material Notes: VESTAMID® DX9325 BK E70352 is a glass fiber-reinforced, PA 612 molding compound. The material contains about 40% glass fiber, an ageing protective agent and processing aid for a fast and even form filling. VESTAMID® DX9325 BK E70352 is especially suitable for the production of plastic and rubber composites. Parts of VESTAMID® DX9325 BK E70352 can be co-vulcanized with EPDM-rubbers without using any adhesives or adhesion promoters ("direct-bonding to rubber"). Because of its semi-crystalline morphology VESTAMID® DX9325 BK E70352 provides an excellent chemical resistance, e. g., against greases, oils, fuels and hydraulic fluids. VESTAMID® DX9325 BK E70352 is supplied as cylindrical pellets ready for processing in moisture-proof bags. Very important are predrying conditions. The material has to be handle as plasticized PA 612. The drying temperature should be not more than 80°C and the drying time at this temperature not more than 4h. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Automotive and Mobility, Industry and Engineering
Processing: Injection molding
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Glass fibers, Release agent
Applications: Electrical and Electronical, Encapsulation, General purpose
Processing: K&K process
Special Characteristics: High impact strength, Semi-crystalline, Light-stabilized, High heat resistant
Features: Good adhesion
Color: Black
Additives: Antioxidant agent, Release agent, Heat stabilizer, Processing aids
Chemical Resistance: Solvent resistance, Oil resistance, Fuel resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.00200 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.00700 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 160 MPaISO 527
Tensile Strength 160 MPaISO 527
Elongation at Break 4.40 %ISO 527
Tensile Modulus 10300 MPaISO 527
Flexural Strength 255 MPaat conv. Deflection; ISO 178
 265 MPaISO 178
 265 MPaat break; ISO 178
Flexural Modulus 10700 MPaISO 178
Flexural Strain at Break 4.00 %at flexural strength; ISO 178
 4.00 %ISO 178
Charpy Impact Unnotched 100 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eU
 104 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eU
Charpy Impact, Notched 16.0 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 60.0 °C
 260 °CInjection Molding; ISO 294
Mold Temperature 80.0 °CInjection Molding; ISO 294
 80.0 °C
Injection Velocity 200 mm/secInjection Molding; ISO 294
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7895 / 325027

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.