MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot CABELEC® CC6495 PS, Conductive Compound
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Product highlights: CABELEC CC6495 conductive concentrate is an electrically conductive concentrate made from a carefully selected carbon black finely dispersed in polystyrene resins. Its electrical and mechanical properties are not dependent on atmospheric conditions; however, they depend on the type and level of dilution of the resin used and the processing conditions. Unlike standard conductive compounds, which have very limited dilution potential, CABELEC CC6495 conductive concentrate can be diluted with a high quantity of natural resin. This allows users of CABELEC CC6495 conductive concentrate to benefit from the versatility of this product and from the enhanced physical properties due to higher levels of dilution resin. The specific carrier resin of CABELEC CC6495 conductive concentrate allows dilution with recycled polystyrene while maintaining good mechanical properties.

Key applications: CABELEC CC6495 conductive concentrate can be used in extrusion applications such as plain sheets thermoformed for electronics packaging, where it is desirable to mitigate the hazard of electrostatic discharge.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Melt Flow 4.5 g/10 min
@Load 230 kg,
Temperature 21.6 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 21 %400µm thick extruded specimens; ISO 527
Flexural Modulus 1970 MPainjection molded specimens; ISO 178
Izod Impact, Notched (ISO) 9.10 kJ/m²injection molded specimens; ISO 180A
Film Tensile Strength at Break, MD 20.0 MPa400µm thick extruded specimens; ISO 527
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 - 210 °CExtrusion
Drying Temperature 80.0 °C
Dry Time 2.00 - 3.00 hour
 
Descriptive Properties
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT060 / 315795

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.