MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kazanorgsintez NMPE-3 Low-Molecular Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Notes: Low-molecular polyethylene of high pressure polyethylene production.

Application: Designed for use in the rubber industry, building industry, and other fields. Can also be used as component parts of compositions.

Information Provided by Kazanorgsintez

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.50 %<= 0.50 %
Viscosity 320 - 7400 cP320 - 7400 cP
Ash <= 0.10 %<= 0.10 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 90.0 - 105 °C194 - 221 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 90.0 - 105 °C194 - 221 °F
 
Descriptive Properties
AppearanceWaxen mass or slipcast blocks of pieces of different size from light-gray to brown colors

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
Lubrizol Advanced Materials Pearlbond® Eco D900 Thermoplastic Polyurethane

PKAZAN069 / 127388

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.