MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Materion Wambraze™ WB850 Solder  (discontinued **)
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic devices. All Williams solder alloys and gold brazing alloys are available in a variety of shapes and forms, including ribbon, preform, rod, ring, wire, and custom shapes. Powders are available in select WAMBRAZE™ alloys.

Trace Impurities for Brazing Alloys:

  • C: 50 ppm max
  • P and Pb*: 20 ppm max
  • Ca*, Cd*, Cs*, Li*, Mg*, Na*, Rb*, S*, Sb*, Se*, Sr*, Te*, Ti*, Zn*: each 10 ppm max
  • Total* 100 ppm max
  • Hg: None detected

Information provided by Williams Advanced Alloys

Former product of Williams Advanced Alloys. Williams Advanced Alloys is now a part of Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 750 - 850 °C1380 - 1560 °F
Solidus 750 °C1380 °F
Liquidus 850 °C1560 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 28 %28 %
Manganese, Mn 5.0 %5.0 %
Nickel, Ni 2.0 %2.0 %
Silver, Ag 65 %65 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Materion C118 Electrical Contact Alloy
Indium Corp. Indalloy 217 Silver Solder Alloy
Indium Corp. Indalloy 216 Silver Solder Alloy
Indium Corp. Indalloy 215 Silver Solder Alloy

NWILL22 / 19910

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.