Homopolymer Features: - Easy processability
- Moderate toughness
- Good heat sealing latitude
Additives: Applications: - Industrial packaging
- Liners
- Blends with LLDPE
Film properties are typical of blown film extruded on a 1.5" extruder with 3" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.United States: NOVAPOL LF-0219-A resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 2.1, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitation that it may not be used in articles used for packing or holding food during cooking. NOVA Chemicals polyethylene resins are biologically and chemically inert. Information provided by NOVA Chemicals® |