MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Angst+Pfister APSOplast® PE-HMW High Molecular Weight Hard PE-HMW (PE-500)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: PE-HMW, also often called PE-500, is more rigid and harder than hard PE. The molecular mass (weight) of the material is around 500 000 g/mol. This type has a good combination of rigidity, toughness, mechanical damping ability, and wear resistance. It is also very suitable for welding processes.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 0.950 g/cc>= 0.0343 lb/in³DIN EN ISO 1183-1
Moisture Absorption <= 0.0100 %<= 0.0100 %50 % r.h.; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 65 - 6765 - 67DIN EN ISO 868
Ball Indentation Hardness 50.0 MPa7250 psiDIN EN ISO 2039-1
Tensile Strength, Yield >= 26.0 MPa>= 3770 psi50 mm/min; DIN EN ISO 527
Elongation at Break >= 350 %>= 350 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity >= 1.10 GPa>= 160 ksi1 mm/min; DIN EN ISO 527
Charpy Impact, Notched 2.50 J/cm²11.9 ft-lb/in²ISO 11542-2
Coefficient of Friction 0.10 - 0.150.10 - 0.15ASTM D 1894
Abrasion 400400PE-UHMW, natural = 100%, (Sand-Slurry-Test); ISO 15527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
Dielectric Strength 45.0 kV/mm1140 kV/inIEC 60243
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 - 200 µm/m-°C83.3 - 111 µin/in-°FDIN 53752
Thermal Conductivity 0.410 W/m-K2.85 BTU-in/hr-ft²-°F
Melting Point 133 - 136 °C271 - 277 °FISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C176 °Flong term
Flammability, UL94 HBHB
 
Descriptive Properties
Colornatural (white)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP004 / 250502

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.