Pro-fax 8623 very high impact polypropylene copolymer is available in pellet form. This resin is typically used in extrusion and injection molding applications and offers excellent cold temperature impact resistance. ASTM and ISO-based versions of the technical data sheet are available for Pro-fax 8623. Availability: North America Application: Automotive Parts; Opaque Containers Market: Automotive Processing Method: Injection Molding; Sheet and Profile Extrusion; Thermoforming Attribute: Low Temperature Impact Resistance Information provided by LyondellBasell. |