MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Ultramid® A 218 V30 Black 21NS Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Product Description: Ultramid® A 218 V30 Black 21NS is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. European Railways Certifications _ EN 45545-2 NC; European Railways Certifications _ EN 45545-2 NC.

Availability: Africa & Middle East; Asia Pacific; North America

Filler/Reinforcement: Glass Fiber, 30% Filler by Weight

Additive: Heat Stabilizer

Features: Heat Stabilized

Agency Ratings: EC 1907/2006 (REACH); EN 45545

RoSH Compliance: RoSH Compliant

Appearance: Black

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66-GF30

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183
Maximum Moisture Content 0.200.20
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 135 MPa19600 psiISO 527-2
Elongation at Break 7.0 %7.0 %ISO 527-2
Tensile Modulus 7.52 GPa1090 ksiISO 527-1
Flexural Strength 215 MPa31200 psiISO 178
Flexural Modulus 6.40 GPa928 ksiISO 178
Izod Impact, Notched (ISO) 18.1 kJ/m²8.60 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) 65.1 kJ/m²31.0 ft-lb/in²ISO 180
Charpy Impact Unnotched 8.40 J/cm²40.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.49 J/cm²7.10 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 62631-3-2
Dielectric Constant 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 29.1 kV/mm
@Thickness 2.00 mm
740 kV/in
@Thickness 0.0787 in
IEC 60243-1
Dissipation Factor 0.11
@Frequency 100 Hz
0.11
@Frequency 100 Hz
IEC 62631-2-1
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 280 °C518 - 536 °F
Middle Barrel Temperature 275 - 285 °C527 - 545 °F
Front Barrel Temperature 280 - 290 °C536 - 554 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2103 / 310796

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.