MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Chase Electronic Coatings HumiSeal® UV500 Acrylic Conformal Coating
Categories: Polymer; Thermoset

Material Notes: HumiSeal® UV500 is a high solids UV dual cure elastomeric acrylate conformal coating. HumiSeal® UV500 exhibits excellent flexibility, moisture resistance and electrical insulation properties as well as good chemical resistance. The formulation allows chemical stripping using a dedicated stripper. HumiSeal® UV500 is tack free after exposure to UV light and the secondary moisture cure mechanism will fully cure any unexposed areas of the coating within 7 days at ambient conditions. Cured HumiSeal® UV500 has a higher flexibility compared to other UV curable conformal coatings, giving improved performance in thermal cycling tests. The coating fluoresces under UV light to allow coating inspection and can be applied by all selective coating equipment. HumiSeal® UV500 is recognized under UL File Number E105698.

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 - 1.10 g/cc0.0361 - 0.0397 lb/in³
Solids Content >= 98 %>= 98 %
Viscosity 275 - 375 cP275 - 375 cPFed-Std-141, Meth. 4287
Thickness 25.0 - 125 microns0.984 - 4.92 milRecommended coating
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 0.000400 GPa
@Temperature 25.0 °C
0.0580 ksi
@Temperature 77.0 °F
DMA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.00e+12 ohm-cm8.00e+12 ohm-cmASTM D257
Surface Resistance 8.90e+10 ohm8.90e+10 ohmIPC J-STD-004 (mod.)
 2.00e+11 ohm2.00e+11 ohmASTM D257
Insulation Resistance 1.60e+10 ohm1.60e+10 ohmMoisture; MIL-I-46058C
 4.50e+11 ohm4.50e+11 ohmMIL-I-46058C
 
Thermal PropertiesMetricEnglishComments
CTE, linear  137 µm/m-°C
@Temperature <=-43.0 °C
76.1 µin/in-°F
@Temperature <=-45.4 °F
Below Tg; TMA
 311 µm/m-°C
@Temperature >=-43.0 °C
173 µin/in-°F
@Temperature >=-45.4 °F
Above Tg; TMA
Thermal Conductivity 0.505 W/m-K3.50 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg -43.0 °C-45.4 °FDSC
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 23.0 °C
6.00 Month
@Temperature 73.4 °F
DOM
 
Descriptive Properties
Dielectric Withstand>1500 Vper MIL_I_46058C
Fungus ResistancePassesIPC-TM-650 2.6.1.1
Resistance to ChemicalsGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Synthos XZ 94466.00 Butadiene Acrylate
Evonik EUDRAGIT® RS 30 D Copolymer

PCHAS921 / 239782

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.