MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECAMID 66 GF30 natural Nylon 66, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes:
  • very good mechanical strength
  • high heat deflection temperature
  • high stiffness
  • high strength
  • excellent wear properties
  • high fatigue strength
  • resistant to many solvents
  • high creep resistance
Target Industries:
  • power engineering
  • gear manufacturing
  • automotive industry
  • conveyor technology
  • mechanical engineering
  • construction industry
  • others

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³
Moisture Absorption 0.300 %0.300 %saturation; ASTM D570
 0.250 %
@Time 86400 sec
0.250 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8888ASTM D 785
Hardness, Rockwell R 117117ASTM D 785
Tensile Strength, Yield 84.1 MPa12200 psiASTM D 638
Elongation at Break 10 %10 %ASTM D 638
Modulus of Elasticity 4.14 GPa600 ksiASTM D 638
Flexural Strength 134.96 MPa19575 psiASTM D 790
Flexural Modulus 4.83 GPa700 ksiASTM D 790
Compressive Yield Strength 117 MPa
@Strain 10 %
17000 psi
@Strain 10 %
ASTM D 695
Compressive Strength 29.6 MPa
@Strain 1 %
4300 psi
@Strain 1 %
ASTM D 695
Compressive Modulus 3.10 GPa450 ksiASTM D 695
Izod Impact, Unnotched 0.400 J/cm0.750 ft-lb/inASTM D 256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmASTM D 257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 48.6 µm/m-°C27.0 µin/in-°FASTM D 696
Specific Heat Capacity 1.26 J/g-°C0.300 BTU/lb-°F
Thermal Conductivity 0.391 W/m-K2.71 BTU-in/hr-ft²-°F
Melting Point 259 °C499 °F
Maximum Service Temperature, Air 110 °C230 °FLong Term
 170 °C338 °FIntermittent
 
Descriptive Properties
Colorgrey-white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8168 / 319096

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.