MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
EOS PA 640-GSL Nylon 12, Glass Bead Filled, Carbon Reinforced
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Glass Bead Filled

Material Notes: This dark gray PA 12 material is filled with both hollow glass beads and carbon fibers. This makes it exceptionally temperature-resistant and rigid, but also very light.

Highlights:

  • Sharp, dark gray appearance
  • Excellent strength to weight ratio properties
  • Cost effective, requiring 10% less material per build
  • Excellent surface finish and detail
Applications:
  • Aerospace/UAV components
  • Athletic equipment
  • Motor sports and racing
  • Ideal for applications requiring a balance of strength and lighter weight without sacrificing dimensional stability and surface finish

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.370 g/ccASTM D1895
Density 0.820 g/ccSintered Part; ASTM D792
Particle Size 55 µmD50, Average
 35 - 100 µmD10-D90, Particle
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 33.0 MPaZ; ASTM D638
 49.0 MPaXY; ASTM D638
Elongation at Break 3.0 %XY; ASTM D638
 3.0 %Z; ASTM D638
Tensile Modulus 1.945 GPaZ; ASTM D638
 3.816 GPaXY; ASTM D638
Flexural Modulus 4.313 GPaZ; ASTM D790
 5.04 GPaXY; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 180 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 170 °CASTM D648
 
Descriptive Properties
ColorDark gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEOS911 / 280571

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.