Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advantages over many other materials.Specific Notes for this Grade: Standard injection grade modified with molybdenum disulphide. For paired sliding parts operating under high surface pressure loading at low sliding speed. Low stick-slip.Information provided by Celanese Corporation. |