System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Daikin NEOFLON® RP-5000AS Tubing Grade EFEP
Categories:
Polymer
;
Thermoplastic
;
Fluoropolymer
;
ETFE/ECTFE
;
Fluorocarbon ETFE/ECTFE, Molded/Extruded
Material Notes:
Neoflon® EFEP RP-5000AS, a functionalized and conductive EFEP, was developed primarily for tubing extrusion. It can be coextruded with other resins such as polyamides directly. It has excellent processability.
Information provided by Daikin.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.73
-
1.79
g/cc
ASTM D-792
Melt Flow
2.5
-
7.5
g/10 min
@Temperature 265 °C
ASTM D-7472
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
29.0
-
50.0
MPa
ASTM D-7472
Elongation at Break
>= 350 %
ASTM D-7472
Electrical Properties
Original Value
Comments
Surface Resistivity per Square
9000
ohm
Thermal Properties
Original Value
Comments
Melting Point
190
-
200
°C
ASTM D-7472
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Daikin NEOFLON® RP-4020 Extrusion/Molding Grade EFEP
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU)
Daikin NEOFLON® RP-4040 EFEP Pellets
Zeus EFEP Tubing
Daikin NEOFLON® EP-7000 Tubing Grade ETFE
PDAIJ9935 / 210006
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.