MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Krytox® NRT 8906 PFPE Lubricant
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE); PTFE Gellant

Material Notes: NRT 8906 provides excellent lubrication options for valves, regulators, seals, and pump and motor bearings at a wide range of operating conditions.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Performance Lubricants, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.95 g/ccOil
Volatiles <= 1.0 %
@Temperature 121 °C,
Time 79200 sec
Oil Volatility; ASTM D972
 <= 5.0 %
@Temperature 204 °C,
Time 79200 sec
Oil Volatility; ASTM D972
Kinematic Viscosity 4.0 cSt
@Temperature 204 °C
Base Oil; ASTM D445
Kinematic Viscosity at 40°C (104°F) 240 cStBase Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 25 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -36.0 °C
 
Descriptive Properties
AppearanceWhite, creamy consistency
Standard NLGI Penetration Grade2
ThickenerPTFE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Krytox® NRT 8904 PFPE Lubricant
Chemours Krytox® CORR 226 FG PFPE Corrugator Grease
Chemours Krytox® XHT-BD Performance PFPE Lubricant
Chemours Krytox® 1506XP Vacuum Pump Fluid with Antirust Protection
Chemours Krytox® 1506 Vacuum Pump Fluid

WDUPJ928 / 162462

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.