Product Description: Dow DMDA-8907 HEALTH+™ HDPE is produced via UNIPOL™ Process Technology from Dow and is intended for use in injection molded medical device applications. This resin has been designed to provide excellent processability for molders and to meet the requirements of devices requiring impact strength and environmental stress crack resistance. Main Characteristics:- Good environmental crack resistance
- Excellent toughness
- Gamma stable
- Low extractables
Complies with: US FDA 21 CFR 177.1520©3.2a; EU, No 10/2011; Canadian HPFB No Objection; USP XXI Class VI; Drug Master File Listing. Consult the regulations for complete details.Availability: North America Additive: Antiblock: No; Processing Aid: No; Slip: No Agency Ratings: DMF; EU No 10/2011; FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection; UL 94; USP 23 Form: Pellets Processing Method: Cast Film; Injection Molding Information provided by The Dow Chemical Company |