MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Pebax® 5533 SN 70 BLACK Polyether Block Amide (PEBA) (Dry)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyether Block Amide (PEBA)

Material Notes: POLYETHER BLOCK AMIDE (PEBA) Hardness 60 shore D Black antistatic grade Applications: Tube extrusion.

Information provided by Arkema.

Key Words: Thermoplastic Elastomer, TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccISO 1183
 1.09 g/ccCond.; ISO 1183
Water Absorption 1.2 %Dry; Sim. to ISO 62
Moisture Absorption 0.500 %Dry; Sim. to ISO 62
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60
@Time 15.0 sec
Dry; ISO 7619-1
Tensile Strength, Yield 17.0 MPaCond.; ISO 527-1/-2
 18.0 MPaDry; ISO 527-1/-2
Elongation at Break >= 50 %Dry; ISO 527-1/-2
 >= 50 %Cond.; ISO 527-1/-2
Elongation at Yield 31 %Dry; ISO 527-1/-2
 36 %Cond.; ISO 527-1/-2
Tensile Modulus 298 MPaCond.; ISO 527-1/-2
 305 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched 18.0 kJ/m²
@Temperature -30.0 °C
Cond.; ISO 179/1eA
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.10e+7 ohm-cmDry; IEC 60093
Surface Resistance 5500 ohmCond.; IEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 220 µm/m-°CDry; ISO 11359-1/-2
Melting Point 159 °C10°C/min; Dry; ISO 11357-1/-3
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection Molding; ISO 294
Mold Temperature 60.0 °CInjection Molding; ISO 10724
Injection Velocity 200 mm/secInjection Molding; ISO 294
Hold Pressure 30.0 MPaInjection Molding; ISO 294
 
Descriptive Properties
ConductiveYes
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
Processing MethodsCasting
 Film Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Thermoforming
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Pebax® 5533 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 5533 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 6333 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® 3533 SA 01 MED Polyether Block Amide (PEBA)

PARKG519 / 25770

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.