MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Colour Image Plastic Compound Loyblend® TA-1300 PC/ABS Polymer alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: Product Description: Loyblend® TA-1300 is a general purpose injection molding PC/ABS alloy compound. This grade offers good low temperature impact resistance, thermal and dimensional stability.

Features:

  • Good low temperature impact resistance
  • Thermal stability with high rigidity
  • Dimensional stability
  • Flow ability
Uses:
  • Electrical/electronic applications
  • Automotive applications
  • Business equipment
Forms:
  • Pellets
Processing Method:
  • Injection Molding

Information provided by Colour Image Plastic Compound Sdn Bhd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm
@Thickness 3.20 mm
0.0055 - 0.0075 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 17 g/10 min
@Load 2.16 kg,
Temperature 260 °C
17 g/10 min
@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength 49.0 MPa7110 psiASTM D638
Elongation at Break 114 %114 %ASTM D638
Tensile Modulus 2.38 GPa345 ksiASTM D638
Flexural Strength 80.0 MPa11600 psiASTM D790
Flexural Modulus 2.196 GPa318.5 ksiASTM D790
Izod Impact, Notched 5.70 J/cm10.7 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
@Thickness 4.00 mm
205 °F
@Thickness 0.157 in
Unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 240 °C410 - 464 °F
Middle Barrel Temperature 220 - 250 °C428 - 482 °F
Front Barrel Temperature 230 - 260 °C446 - 500 °F
Nozzle Temperature 240 - 260 °C464 - 500 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOLO099 / 265991

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.