MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ PFE 80Z Peroxide Cure Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ Dyneon™ Peroxide Cure Perfluoroelastomer PFE 80Z is a technically advanced peroxide curable perfluoroelastomer. This product is designed to have improved acid resistance and lower metal ion extractables making it ideal for wet process electronics manufacturing such as semiconductor and flat panel display. It is classified as FFKM per ASTM D1418. Its fully fluorinated back bone structure provides a very broad chemical and thermal stability.

    Features and Benefits:
  • Ideal for wet chemical, fluid handling, cleaning and chemical etching processes and for semiconductor manufacturing
  • Good acid resistance
  • Upper use temperature of 200°C
  • Very low metal ion content with low extractables in a wide range of chemicals
  • Peroxide curable FFKM

Information provided by the Dyneon division of 3M.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.00 g/cc
Mooney Viscosity 80
@Temperature 121 °C
ML 1+ 10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 72Press Cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 200°C; ASTM D2240
Tensile Strength at Break 11.0 MPaPress Cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 200°C; ASTM D412
Elongation at Break 230 %Press Cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 200°C; ASTM D412
100% Modulus 0.00480 GPa
@Strain 100 %
Press Cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 200°C; ASTM D412
Compression Set 49 %
@Treatment Temp. 200 °C,
Time 252000 sec
Method B, -214 O-rings, Aged 70 Hours, 25% Deformation; ASTM D395
 69 %
@Treatment Temp. 200 °C,
Time 605000 sec
Method B, -214 O-rings, Aged 168 Hours, 25% Deformation; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Brittleness Temperature -35.0 °C
Transformation Temperature -2.00 °CTR10
 
Descriptive Properties
ColorOff White
FormSlab
MH, Maximum Toque11.9 Inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
ML, Minimum Torque2.0 Inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t2, Time to 2 Inch-lb Rise from Minimum0.8 Minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t'50, Time to 50% Cure1.1 Minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t'90, Time to 90% Cure2.7 Minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akzo Nobel Trigonox® KSM Peroxide Cure Agent
DuPont Mobility and Materials Hypalon® 20 Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound
DuPont Mobility and Materials Hypalon® 30 Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound
DuPont Mobility and Materials Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound
Greene Tweed CHEMRAZ® 505 Perfluoroelastomer

PDYL9964 / 129982

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.