Molding Grade PCFR w/ UV and Release, All Colors. NCNB (Non-chlorinated & Non-Brominated) FR PC . Polycarbonate (PC), furnished as pellets, Non-Chlorine & Non-Bromine (All Colors). May be used to produce molded or extruded articles or as a component of other industrial products.Information provided by Star Plastics. |