MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Free Form® Sculpt Epoxy Putty
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Overview: Free Form® SCULPT is a two part sculpt-able epoxy clay that requires no firing and will self-cure in a short time to an extremely hard and durable state with virtually no shrinkage. SCULPT is 30% lighter than similar products and holds vertical surfaces better. Users can sculpt larger, stronger pieces with more control over weight distribution. Free Form SCULPT has an ultra fine particle size that gives the user the ability to sculpt finer detail with better precision using tools or shaping by hand. A mirror-like, gloss finish can be achieved by smoothing SCULPT with water before it cures. Maximum Usability - Just Add Water; you can change the consistency and workability of Free Form® SCULPT by adding water when mixing A+B components. Putty surface can be smoothed with water while sculpting. Parts A & B are mixed in equal amounts by hand. Working time is a long 1.5 hours and Free Form® SCULPT cures overnight to a hard, rigid epoxy that is very strong and waterproof. SCULPT is easily colored by adding UVO™ or IGNITE™ colorants to create marble or other effects. Cured putty is easily painted with acrylic paints. Free Form® SCULPT does not contain crystalline silica (which is a known carcinogen). It can be safely sanded, shaped, and painted. Used as a repair adhesive, Free Form® SCULPT will bond to itself and a variety of surfaces including wood, metal, glass, stone, and concrete. Free Form® SCULPT will even cure under water.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D-1475
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080ASTM D-2240
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 65.0 °C149 °FHeat Deflection Temperature; ASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourovernight
Pot Life 90.0 min
@Thickness 25.4 mm
90.0 min
@Thickness 1.00 in
ASTM D-2471
 
Descriptive Properties
ColorGrey
Mix Ratio1A:1Bby volume
 1A:1Bby weight
Mixed ViscosityPutty
Specific Volume20.7[in3/lb], ASTM D1475

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN212 / 296913

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.