Silver Zinc Ink C70709D18 is designed as a screen printing ink for coating PTC ceramics as a one part formula, and does not need a top coat of silver as a protection layer. The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. Information provided by Gwent Electronic Materials Ltd. |