MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LATI Latamid 6 E02 PA 6, Impact modified
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Polyamide 6 (PA6). Toughened. Good impact resistance.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/cc
Linear Mold Shrinkage, Flow 0.0115 - 0.0145 cm/cm
Linear Mold Shrinkage, Transverse 0.0125 - 0.015 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break >= 100 %
@Temperature 23.0 °C
 >= 100 %
@Temperature 60.0 °C
 >= 100 %
@Temperature 90.0 °C
 >= 100 %
@Temperature 120 °C
 >= 100 %
@Temperature 150 °C
Elongation at Yield 5.0 %
@Temperature 23.0 °C
Tensile Modulus 150 MPa
@Temperature 150 °C
 200 MPa
@Temperature 120 °C
 320 MPa
@Temperature 90.0 °C
 450 MPa
@Temperature 60.0 °C
 2000 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched NB
@Temperature 23.0 °C
 NB
@Temperature -20.0 °C
Charpy Impact, Notched 100 kJ/m²
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 55.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
Vicat Softening Point 175 °C
@Load 5.00 kg
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 250 °C
Mold Temperature 60.0 - 70.0 °C
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Latamid 66 E21 PA 66, Impact Modified
Ensinger Tecamid® HS Nylon (PA)
Edinburg Plastics HTT605 PA 6 Impact Modified
Edinburg Plastics HGT605 PA 6 Impact Modified
Global EPP PA 6C HS BLUE Cast Polyamide 6 + UV and Heat Stabilizers

PLATH9683 / 177379

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.