MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI ALLEN® 5200WHG PC/ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: ALLEN® 5200WHG Sheet has an excellent weatherable performance and property retention with high impact strength, high heat deflection, and stiffness.

ALLEN® 5200WHG has been tested under laboratory conditions and has achieved a UL94 HB rating at 0.060 in (1.52mm) and above and meets the requirements of Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302).

Suggested Application:

  • Engine Covers
  • Heavy Truck
  • Recreational Vehicles
  • Bus/Van
  • Auto After-Market
  • Agriculture/Construction Equipment
Features:
  • Wide range of colors
  • Excellent physical property retention
  • Excellent low temperature impact
  • High heat deflection temperature
  • Improved performance over ABS
  • High modulus (Increased stiffness)

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccASTM D792
Water Absorption 0.170 %equilibrium; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 111ASTM D785
Tensile Strength 48.0 MPaASTM D638
Tensile Modulus 2096 MPaASTM D638
Flexural Strength 80.0 MPa
@Strain 5.00 %
ASTM D790
Flexural Modulus 2230 MPaASTM D790
Compressive Yield Strength 59.2 MPaASTM D695
Bearing Yield Strength <= 228.2 MPaASTM D953
 27.9 MPa
@Strain 4.00 %
ASTM D953
Shear Strength 54.0 MPaASTM D732
Izod Impact, Notched 438.3 J/m
@Temperature -29.0 °C
ASTM D256
 523.9 J/m
@Temperature 23.0 °C
ASTM D256
Gardner Impact 50.1 J
@Temperature 23.0 °C
Drop Dart Impact, GE; ASTM D5420
 59.0 J
@Temperature -29.0 °C
Drop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 21.7 kV/mmoil; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 77.0 µm/m-°CASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 122 °Cannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 101 °Cannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.52 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSEKIS535 / 325275

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.