MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Ineos H35Z-02 Nucleated and antistated homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: H35Z-02 is a high flow rate, nucleated and antistatic homopolymer designed for injection molding applications. Typical applications include consumer products, house wares, medical components and thin-walled rigid packaging. Benefits include high flow rate, fast cycle times, good molding performance in thin-wall parts, low static charge and improved toughness. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

Information provided by INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
35 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 106106ASTM D785
Tensile Strength, Yield 38.0 MPa5510 psi2 in/min; ASTM D638
Elongation at Yield 9.0 %9.0 %2 in/min; ASTM D638
Flexural Modulus, 1% Secant 1700 MPa247000 psiASTM D790A
Izod Impact, Notched (ISO) 2.75 kJ/m²1.31 ft-lb/in²ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 117 °C243 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Gloss 89 %89 %@ 60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21CFR 177.1520

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINEOS852 / 291458

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.