MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Aperam Superimphy® 276 Bar-Corrosion application
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: SY276 is a Ni alloy, with high Mo and Cr level, and low carbon content. This composition offers a excellent corrosion resistance in a wide range of aggressive environments.

Applications:

  • Chemical industries (sulfuric acid, phosphoric acid)
  • Pulp and paper industry
  • Pollution control (waste treatment)
  • Oil and gas, petrochemicals
  • Heat exchanger, evaporators
Standards related to these applications : ASTM B564, ASTM B574 and NACE MR0175

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al >= 4.5 %>= 4.5 %
Chromium, Cr 14.5 - 16.5 %14.5 - 16.5 %
Cobalt, Co <= 2.5 %<= 2.5 %
Iron, Fe 4.0 - 7.0 %4.0 - 7.0 %
Molybdenum, Mo 15 - 17 %15 - 17 %
Nickel, Ni 59.5 - 63.5 %59.5 - 63.5 %
Tungsten, W <= 3.0 %<= 3.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy C-276
MetalTek MTEK CW-12MW Cast UNS N30002 Severe Corrosion and Heat Resistant Alloy
HP Alloys Alloy C-276, 10% Cold Worked
Haynes Hastelloy® C-276 alloy, solution heat treated flat products
Haynes 214® Alloy Sheet

NPERA020 / 194809

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.