MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Versalis Sinkral® E 332 ABS Resin
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Sinkral E 332 is a medium heat injection molding grade offering good flow and good impact resistance together with an excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-ABS 1, MGN, 105-08-16-25.

Applications: Thanks to a low Yellow Index and color constancy, it is suitable for self-coloring, mainly in the automotive industry (internal trim parts)

Grade available in natural color only. Suitable masterbatches could be recommended for self-coloring. The composition of this grade meets European Regulations for packaging in contact with foodstuffs.

Information provided by Polimeri Europa

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Water Absorption 0.30 %24 hours - 23°C; ASTM D 570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
Melt Flow 10 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 111ISO 2039/2
Tensile Strength, Yield 40.0 MPa50 mm/min; ASTM D 638
Elongation at Break 75 %50 mm/min; ASTM D 638
Flexural Strength 62.0 MPa2 mm/min; ASTM D 790
Flexural Modulus 2.20 GPa2 mm/min; ASTM D 790
Izod Impact, Notched 85.0 J/m
@Thickness 3.20 mm,
Temperature -40.0 °C
ISO 180/4A
 90.0 J/m
@Thickness 3.20 mm,
Temperature -20.0 °C
ISO 180/4A
 115 J/m
@Thickness 3.20 mm,
Temperature 0.000 °C
ISO 180/4A
 190 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ISO 180/4A
Izod Impact, Notched (ISO) 8.00 kJ/m²
@Thickness 4.00 mm,
Temperature -40.0 °C
ISO 180/1A
 15.0 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -40.0 °C
DIN 53453
 NB
@Temperature 23.0 °C
DIN 53453
Charpy Impact, Notched 1.20 J/cm²
@Temperature 23.0 °C
DIN 53453
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+14 ohmDry; IEC 60093
Dielectric Constant 3.1
@Frequency 1000 Hz
Dry; IEC 60250
Dielectric Strength 30.0 kV/mmDry; IEC 60243
Dissipation Factor 0.015
@Frequency 1000 Hz
dry; IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature 20.0 °C
ASTM D 696
Thermal Conductivity 0.170 W/m-KASTM C 177
Deflection Temperature at 1.8 MPa (264 psi) 103 °C120°C/h; ASTM D 648
Vicat Softening Point 104 °C50 N - 120°C/h; ISO 306/B120
 109 °C10 N - 120°C/h; ISO 306/A120
Flammability, UL94 HB
@Thickness 1.50 mm
Glow Wire Test 650 °C
@Thickness 3.00 mm
IEC 60695-2-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 280 °C
Mold Temperature 40.0 - 70.0 °C
Drying Temperature 80.0 °CNo venting in an air circulating oven
Dry Time 2 - 4 hourNo venting in an air circulating oven

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Sinkral® F 332 ABS Resin
Stratasys® ABS-M30i
GEHR Plastics ABS Acrylonitrile Butadiene Styrene

PENJ53 / 35928

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.