VESTAKEEP® i4 3DF-T is a filament extruded from natural colored, high viscosity VESTAKEEP® i4 G polyether ether ketone (PEEK) resin. The material is a testing grade designed for research, development and process optimization only. It must not be used for medical devices. Dry properties listed below Industrial Sector: Medical Devices, 3D Printing Processing: 3D Printing Delivery form: (Mono)filament Optics: Opaque Resistance to: Heat (thermal stability), Hydrolysis / hot water, Oil / fuels Conformity: Medical application Additives: Unfilled Applications: Monofilament Processing: Fused deposition molding, Additive manufacturing Special Characteristics: Semi-crystalline, High viscosity, Sterilizable Regulatory: US Pharmacopeia Class VI conformity Color: Natural color Chemical Resistance: Acid resistance, Alkali resistance, Solvent resistance, Grease resistance, Hydrolytically stable, Oil resistance, Oxidation resistance, General chemical resistanceInformation provided by Evonik. |