MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical LUPOY GN5001RFP PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General Purpose

Application: E&E (TV, Navigation Housing)

CAS: 103598-77-2, 9003-56-9 and 181028-79-5

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Maximum Moisture Content 0.020Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 670 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 80 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Yield Strength 1000 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Flexural Modulus 28000 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Izod Impact, Notched 12.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 80.0 °C
UL RTI, Mechanical with Impact 80.0 °C
UL RTI, Mechanical without Impact 85.0 °C
Flammability, UL94 V-0
@Thickness >=1.20 mm
 V-0
@Thickness >=2.50 mm
 V-0
@Thickness >=3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 240 - 265 °CInjection Molding
Middle Barrel Temperature 250 - 270 °CInjection Molding
Front Barrel Temperature 255 - 275 °CInjection Molding
Nozzle Temperature 260 - 280 °CInjection Molding
Melt Temperature 260 - 280 °CInjection Molding
Mold Temperature 70.0 - 90.0 °CInjection Molding
Drying Temperature 85.0 - 95.0 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
Back Pressure 0.00200 - 0.00600 MPaInjection Molding
Screw Speed 40 - 70 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOY GN5001RFT PC/ABS, Halogen Free Flame Retardant
LG Chemical LUPOY GN5001RFD PC/ABS, High Impact
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant

PLAY587 / 148597

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.