MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow ISONATE™ 143L Modified MDI
Categories: Fluid

Material Notes: ISONATE™ 143L modified MDI is a polycarbodiimide-modified diphenylmethane diisocyanate.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.214 g/cc
Viscosity 33 cP
Viscosity Measurement 2.0 - 5.0[cps/mo.] Viscosity growth
Vapor Pressure <= 1.30e-8 bar
 
Chemical PropertiesOriginal ValueComments
Acid Value 0.0020HCl content, %
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 86.0 cal/g
CTE, linear 741 µin/in-°F
@Temperature 20.0 °C
Specific Heat Capacity 1.80 J/g-°C
Thermal Conductivity 0.000300 cal cm/sec-cm²-°C
Boiling Point 314 °C
Decomposition Temperature 230 °C
Flash Point >= 351 °FASTM D93 Closed Cup
 
Descriptive Properties
NCO Content %29.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow ISONATE™ 181 MDI Prepolymer
BASF Lupranate® 219 Isocyanate Modified MDI
TSE Industries Millstab™ P Hydrolytic Stabilizer Additive
Dow PAPI™ 95 Polymeric MDI
3M Novec™ 7000 Engineered Fluid

PDOW1390 / 30608

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.