MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sinvicomp SBF3715 Rigid Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Sinvicomp SBF3715 is a tin-based blown film grade polyvinylchloride resin available in granular form. SBF3715 provide good performance suitable for shrink wrap film. This products resin contains ingredients that are non-toxic and have been approved for food applications by internationally recognized bodies.

Availability: Asia Pacific

Features: Food Contact Acceptable

Form: Pellets

Processing Method: Blow Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 - 1.32 g/cc0.0462 - 0.0477 lb/in³ASTM D792
Melt Flow 17 g/10 min
@Load 21.6 kg,
Temperature 190 °C
17 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070ASTM D2240
Tensile Strength, Yield 31.4 MPa4550 psiASTM D638
Elongation at Break 150 %150 %ASTM D638
Izod Impact, Notched 0.294 J/cm0.550 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 70.0 °C158 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 170 °C320 - 338 °FCompression
 170 - 180 °C338 - 356 °FMixing
Feed Temperature 160 °C320 °F
Nozzle Temperature 180 °C356 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1414 / 237905

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.