This grade has been specially created for parts submitted to tribological stresses. At high PV, wear and friction are very low and this is very important to increase the lifetime of the different components. Having a high tensile, compressive and flexural strength, Meldin® 5000 materials are injection molded into tight-tolerance finished components in simple or complex designs that can exhibit metal-like finishes without expensive machining or secondary operations, and with the advantages of being lighter and corrosion resistant. |