MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Permabond HH040 Pure NSF 61 Approved Anaerobic Retainer
Categories: Polymer; Adhesive; Thermoset

Material Notes: Permabond® HH040 PURE is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure unitizes and retains male and female parts. Thus it prevents their movement relative to each other, eliminating wear, erosion, and pitting. HH040 PURE cures to a tough cross-linked plastic that will prevent the corrosion of mated parts, and provides excellent environmental and temperature resistance.

PERMABOND® HH040 PURE Anaerobic Retaining Compound conforms to all applicable requirements of the NSF/ANSI Standard 61, Drinking Water System Components - Health Effects, as certified by NSF International and the American National Standards Institute. Standard 61 establishes minimum health effects requirements for materials, components, products, or systems that contact drinking water or drinking water treatment chemicals. NSF standards are widely recognized by public health officials, and certified products have been tested and determined to cause no adverse health effects. This allows manufacturers using certified materials to bypass some or all chemical testing when seeking NSF certification.

Features & Benefits:

  • NSF certified drinking water system component
  • Simple one-part system
  • Shaft-hub assemblies can be made with slip fits
  • Expensive press fits can be eliminated
  • High viscosity for maximum gap filling ability
  • Excellent shear strength
  • Superior environmental resistance
  • Thixotropic viscosity allows easy dispensing

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccUncured
Viscosity 5000 cP
@Temperature 25.0 °C
Uncured
Storage Temperature 5.00 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 14.0 MPasteel collar and pin shear; ISO 10123
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 11.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
Thermal Conductivity 0.200 W/m-K
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -65.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 0.0830 hour
@Temperature 23.0 °C
Brass, handling strength
 0.250 hour
@Temperature 23.0 °C
M10 steel, handling strength
 0.500 hour
@Temperature 23.0 °C
Brass, working strength
 1.00 hour
@Temperature 23.0 °C
Zinc, handling strength
 1.00 hour
@Temperature 23.0 °C
M10 steel, working strength
 6.00 hour
@Temperature 23.0 °C
Stainless steel, handling strength
 6.00 - 24.0 hour
@Temperature 23.0 °C
Zinc, working strength
 24.0 hour
@Temperature 23.0 °C
M10 steel, full strength
 
Descriptive Properties
AppearanceColorless to Light AmberUncured
Maximum Gap Fill (mm)0.25
Maximum Thread SizeM30
Strength Retention50% at 150°CRelative to 0°C
 80% at 100°CRelative to 0°C
 93% at 50°CRelative to 0°C
Torque Strength (N m)25M10 steel, break
 37M10 steel, prevail

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPERMA21 / 56129

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.