MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Accella Bayblock® HT Acrylic Coating
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Characterization: Bayblock HT is a technologically advanced, high-solids, alkali resistant, thixotropic,acrylic elastomeric coating.

Properties / Applications: Bayblock HT is formulated for the protection of sprayed-in place polyurethane foam, metal, polyurea, stucco, siding, and concrete. It is a specially formulated adhesion basecoat with plasticizer migration resistance and contrasting color to help achieve proper coverage and accelerated cure.Bayblock HT coating provides an excellent protective membrane that remains flexible even under adverse conditions. Its elongation and tensile strength provides superior resistance to maintenance traffic, weather conditions, and wear. Bayblock HT coating was specifically developed as a protective coating for sprayed polyurethane foam surfaces. The thixotropic nature of Bayblock HT coating permits uniform high build coverage, even on rough, textured or vertical surfaces, without pinholing or sagging. It also has excellent adhesion to a variety of other substrates such as primed wood, primed metal, concrete and masonry. Ponding water conditions should be avoided, if possible, as with any type of roofing material. However, Bayblock HT coating can be used in limited areas with ponded water where a primer is used in conjunction with the coating. As with any product, use of Bayblock HT coating in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Covestro sold their spray polyurethane foam business to Accella in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 57 - 59 %ASTM D2697, by volume
 63 - 67 %ASTM D1644, by weight
Viscosity Measurement 110 - 117KU + 2 (krebs units); ASTM D D562
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2.26 MPa
@Thickness 0.508 mm
ASTM D2370
Elongation at Break 485 %
@Thickness 0.508 mm
ASTM D412
Tear Strength Test 112[psi]; ASTM D624
Peel Strength 2.15 - 6.15 plipeel strength to foam; ASTM C794-D903
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °F
Minimum Service Temperature, Air -30.0 °F
 
Descriptive Properties
ColorGrayBasecoat
 White, gray5400 Topcoat

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Autoclaved aerated concrete, 0.800 g/cc density
Cymat A35620SC 020SS Stabilized Aluminum Foam
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness
Evonik TEGO® Antifoam 5-27 Emulsion
Rogers Arlon CuClad 217 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate

PCOVEST0060 / 201843

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.