MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Master Bond EP21ARHTND-2 Two Component Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Paste consistency
  • Convenient handling
  • Superior temperature resistance
  • Good physical strength properties
Product Description: Master Bond EP21ARHTND-2 is a two component epoxy resin system for high performance bonding, sealing and coating. It has a convenient 100 to 50 mix ratio by weight and is formulated to cure at ambient temperatures, or more quickly at elevated temperatures. Various cure schedules are noted in the chart below, with the optimum cure being overnight at ambient temperature followed by 2-4 hours at 150-200°F. The primary use of this system is for acid resistance, particularly sulfuric and hydrochloric acids. EP21ARHTND-2 has very low linear shrinkage upon cure, is 100% reactive, and contains no solvents or diluents. This system bonds well to a wide variety of substrates including metals, glass, ceramics, rubbers and plastics. It has excellent physical strength properties, notably high tensile strength. It withstands thermal cycling and has a low coefficient of thermal expansion. It is also a robust electrical insulator. EP21ARHTND-2 has a smooth paste consistency that is especially accommodating for a number of applications including the coating of substrates that might be used in tanks and storage containers. Its viscosity makes using it simple and straight forward, as the epoxy will not flow when applied. The service temperature range is -60°F to +400°F. The color of Parts A and B are amber. EP21ARHTND-2 is widely used in aerospace, electronic, electrical, chemical processing, and in other applications where chemical resistance to acids is needed and a non-drip viscosity is helpful.

Product Advantages:

  • Convenient handling, 2:1 mix ratio by weight
  • Smooth paste consistency
  • Good physical strength properties
  • Outstanding chemical resistance, particularly to acids

Information provided by Master Bond, Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75.0 - 85.075.0 - 85.0
Tensile Strength 62.1 - 68.9 MPa9000 - 10000 psi
Adhesive Bond Strength 15.2 - 16.5 MPa2200 - 2400 psilap shear, aluminum to aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 3.80
@Frequency 60 Hz
3.80
@Frequency 60 Hz
Dielectric Strength 17.3 kV/mm
@Thickness 3.17 mm
440 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 - 45.0 µm/m-°C22.2 - 25.0 µin/in-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -51.0 °C-59.8 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 93.3 °C
2.00 - 3.00 hour
@Temperature 200 °F
 1440 - 2880 min
@Temperature 23.9 °C
24.0 - 48.0 hour
@Temperature 75.0 °F
Working Life 30.0 - 50.0 min30.0 - 50.0 minafter mixing, 100 gram batch
Shelf Life 12.0 Month12.0 Monthin original, unopened containers
 
Descriptive Properties
Mixing ratio100:50Part A to B
Optimum cure scheduleOvernight at 75°F followed by 2-4 hours at 150-200°F
ViscositypastePart A
 pastePart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM5801 / 323318

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.